  1. Fresh Cement: If extracted out quickly with Brown Out® at 4 ounces per gallon, fresh cement will usually come out. Cement is highly alkaline.
  2. Once cement has set up and hard, it is much more difficult to remove.
  3. Hardened Cement: Break up the hardened cement with a hammer until it is a fine dust and vacuum. Then extract with Brown Out at 4 ounces per gallon.
  4. To prevent wicking, heavily sprinkle Stain Blotter on area to absorb any material that wicks up.
  5. The customer can vacuum up the Stain Blotter the next day.